Infrared Welding Efficiently Joins Recyclable Acrylic Composites Without
Infrared radiation welding provides a rapid, contamination-free, and fully recyclable joining method for acrylic-based thermoplastic composites, achieving lap shear strengths up to 13.72 megapascals for glass fiber laminates and 9.59 megapascals for carbon fib
Illustrative imageInfrared radiation welding provides a rapid, contamination-free, and fully recyclable joining method for acrylic-based thermoplastic composites, achieving lap shear strengths up to 13.72 megapascals for glass fiber laminates and 9.59 megapascals for carbon fiber laminates without chemical adhesives. In a newly published structural investigation, engineering researchers systematically evaluated how non-contact thermal radiation can soften and fuse polymer matrices in advanced composite assemblies, establishing an energy-efficient alternative to conventional fasteners and thermoset bonding. By directing focused infrared emission onto joint overlap surfaces prior to rapid consolidation in a hydraulic press, the experimental process relies purely on heat-induced macromolecular mobility across the mating interface to establish structural integrity. The resulting mechanical performance demonstrated that glass fiber composite joints achieved 43 percent higher shear strength than carbon fiber joints under identical welding conditions of 150 degrees Celsius and 0.5 megapascals.
The polymeric foundation of the investigated material system is Elium 150, a liquid thermoplastic acrylic resin developed by Arkema that polymerizes at ambient room temperature while retaining the reprocessability of linear macromolecules. Unlike conventional thermosetting resins such as epoxies, vinyl esters, and polyesters, which undergo permanent chemical cross-linking that prevents melting or thermal reshaping, this reactive methyl methacrylate copolymer system combines thermoset-like processing fluidity with the recyclability of thermoplastics. In standard industrial manufacturing, conventional solid thermoplastics demand elevated processing temperatures and exhibit high melt viscosity, which impedes thorough fiber wet-out and necessitates specialized machinery. In contrast, the low initial viscosity of the room-temperature acrylic formulation allows composite fabrication using well-established vacuum infusion infrastructure while retaining high toughness and weldability. Furthermore, polymethyl methacrylate matrices provide practical pathways for circular material recovery, as cured panels can undergo mechanical recycling, thermal pyrolysis for fiber extraction, or chemical solvolysis to dissolve the matrix resin for sustainable structural manufacturing.
To evaluate welding behavior across representative reinforcements, composite laminate plates were fabricated via vacuum-assisted resin transfer molding using Elium 150 resin mixed with 1.2 weight percent Luperox 78 initiator and cured at 25 degrees Celsius. The investigation examined two distinct reinforcement architectures designed to achieve a matched total laminate thickness of approximately 2 millimeters in compliance with ASTM D5868 standards. The carbon fiber laminates comprised five balanced orthogonal plies of polyacrylonitrile-based high-strength carbon fabric possessing a 6k tow structure, an areal weight between 370 and 400 grams per square meter, and an estimated fiber volume fraction of 53 percent. The glass fiber counterparts were fabricated using ten plies of woven E-glass fabric with an areal weight of 200 grams per square meter, yielding an estimated fiber volume fraction of 39 percent. Both reinforcement types retained standard commercial sizing formulations intended for thermoset compatibility, specifically epoxy sizing on carbon fibers and silane sizing on glass fibers, without supplementary chemical grafting or etching treatments.
Establishing a reliable thermal processing window required rigorous calorimetric and thermogravimetric evaluation of the neat polymer and composite laminates to identify the temperature boundaries where fusion occurs without degradation. Differential scanning calorimetry performed under a nitrogen atmosphere at a heating rate of 10 degrees Celsius per minute identified an exothermic curing peak at 82 degrees Celsius, corresponding to methyl methacrylate polymerization, with a reaction enthalpy of 241 joules per gram. Dynamic cooling curves erased thermal history and measured a glass transition temperature of 94.16 degrees Celsius, marking the threshold where the amorphous polymer transitions into a viscous state suitable for molecular interdiffusion. Concurrently, thermogravimetric analysis conducted in synthetic air revealed that thermal degradation onset, defined by a one percent mass loss threshold, occurred at 204 degrees Celsius. Major mass loss of approximately 40 percent took place between 300 and 410 degrees Celsius due to acrylic chain scission. Consequently, experimental welding temperatures were established at 150, 175, and 200 degrees Celsius.
The experimental infrared welding apparatus incorporated a 1000-watt quartz halogen lamp mounted at an adjustable distance above a rigid metal support base. The lamp operated at a color temperature of approximately 2450 Kelvin, converting electrical energy into high-intensity infrared radiation that delivered non-contact electromagnetic thermal energy directly to the targeted composite substrate. Test specimens were machined to standard lap shear dimensions measuring 101.6 millimeters by 25.4 millimeters in accordance with ASTM D5868 specifications. Surface preparation across all welded coupons was restricted exclusively to stripping away peel ply cloth immediately prior to processing, creating a textured, contamination-free topography without applying chemical solvents, mechanical abrasives, or atmospheric plasma treatments. Aluminum foil was carefully wrapped around each specimen to shield non-bonded laminate regions, leaving exposed a standardized bonding window measuring exactly 25.4 millimeters by 25.4 millimeters, equivalent to an effective overlap area of 645.16 square millimeters.
Thermal mapping determined that positioning the quartz halogen lamp at a working distance of 15 centimeters provided controlled heating capable of reaching setpoints of 150, 175, and 200 degrees Celsius within 180 seconds. A one-dimensional thermal conduction model based on the laminate thickness of 2 millimeters and an acrylic composite thermal diffusivity of approximately 10⁻⁷ square meters per second demonstrated a characteristic through-thickness diffusion time of roughly 40 seconds. Holding the target surface temperature for 180 seconds ensured that sufficient thermal energy penetrated the overlapping adherends to induce thorough matrix softening across the mating interface. Following irradiation, stacked specimens were transferred in less than 10 seconds to a hydraulic press, undergoing negligible thermal decay before experiencing sustained consolidation for 10 minutes at preset cooling pressures of 0.4 and 0.5 megapascals.
To benchmark infrared welding performance against conventional adhesive joining, reference coupon sets were fabricated using neat Elium 150 resin mixed with 1.2 weight percent Luperox initiator under identical geometric configurations. Following manual mixing until a color shift from clear to yellow confirmed homogenization, the resin rested for 15 minutes before being applied by brush to both mating surfaces of peel-ply-prepared adherends. The bonded assemblies were clamped in a mechanical press under a constant pressure of 0.2 megapascals at 25 degrees Celsius for two hours, utilizing calibrated shims to maintain a uniform bondline thickness without post-cure heating. In accordance with standardized adhesive testing protocols, bonded coupons were stored under ambient conditions for 24 hours prior to mechanical evaluation to guarantee adequate monomer conversion. Subsequent lap shear testing was conducted using a Shimadzu AG-X universal testing machine fitted with a 50-kilonewton load cell operating at a constant crosshead displacement rate of 13 millimeters per minute, providing direct comparative metrics.
A full factorial two-level design of experiments was executed to systematically isolate the effects of reinforcement type, joining temperature, and consolidation pressure on resultant lap shear strength. The experimental design incorporated 36 randomized trials encompassing eight factorial combinations, three replicates per condition, and twelve center points. Statistical analysis of variance and Pareto charting demonstrated that reinforcement fiber type and joining temperature exerted dominant and statistically significant effects on joint strength, displaying standardized effect sizes of approximately plus 2 for glass fiber, minus 2 for carbon fiber, and minus 2.3 for temperature. Conversely, varying consolidation pressure between 0.4 and 0.5 megapascals generated a negligible effect that lacked statistical significance within the examined processing window. Mathematical modeling established an empirical linear relationship where lap shear strength decreased with increasing temperature while benefiting substantially from glass fiber reinforcement. Multiple-comparison Tukey testing verified that glass fiber laminates exhibited consistently superior shear strength across all test combinations.
Quantitative mechanical testing corroborated statistical predictions, establishing that infrared-welded joints achieved peak performance at a processing temperature of 150 degrees Celsius under 0.5 megapascals of pressure. At this optimal condition, glass fiber joints attained a mean lap shear strength of 13.72 ± 4.76 megapascals, whereas carbon fiber joints reached 9.59 ± 1.60 megapascals. Elevating the welding temperature to 175 and 200 degrees Celsius caused a pronounced reduction in shear strength across all configurations, confirming that approaching the polymer degradation threshold impairs interfacial cohesion. Reference specimens bonded with liquid Elium resin demonstrated superior overall mechanical strength, recording 16.21 ± 1.90 megapascals for glass fiber and 14.22 ± 1.61 megapascals for carbon fiber, matching commercial structural adhesives such as Acralock SA10-60 and Plexus 310.
Post-fracture characterization using a Zeiss EVO MA-15 scanning electron microscope revealed distinctive microscopic failure modes that elucidated the mechanical disparities between reinforcement materials. Adhesively bonded reference specimens exhibited pervasive cohesive failure within the resin layer with plastic deformation and microscopic shear cusps. Similarly, infrared-welded glass fiber joints fabricated at 150 degrees Celsius exhibited predominantly cohesive failure within the consolidated acrylic matrix, accompanied by distinct fiber imprints and polymer anchoring that signaled robust chemical compatibility between silane-sized glass filaments and acrylic resin. In sharp contrast, carbon fiber welded joints exhibited extensive adhesive failure along the fiber-matrix interface, characterized by stripped carbon tows and minimal residual resin coverage. Microscopic inspection revealed that applying 0.5 megapascals of pressure at elevated temperatures induced localized resin leakage and starvation. Because commercial carbon fibers bore epoxy-compatible sizing, interfacial wetting remained suboptimal, indicating that industrial deployment of carbon fiber variants will require dedicated surface functionalization strategies such as compatible sizing, plasma activation, or chemical grafting to enhance interfacial bonding.
Subject of Research: Infrared radiation welding of carbon and glass fiber reinforced acrylic thermoplastic composites
Article Title: Infrared Welding as an Efficient Joining Method for Sustainable Thermoplastic Composites
Article References: de Oliveira Campos, F. M., da Costa, T. B., Di Benedetto, R. M., Barbosa, L. C. M., & Ancelotti Junior, A. C. (2026). Infrared Welding as an Efficient Joining Method for Sustainable Thermoplastic Composites. Applied Composite Materials, 33(2), Article 66. https://doi.org/10.1007/s10443-025-10436-z
Image Credits: AI Generated
DOI: 10.1007/s10443-025-10436-z
Keywords: infrared welding, thermoplastic composites, Elium 150, acrylic resin, lap shear strength, fusion bonding, carbon fiber reinforced polymers, glass fiber composites, vacuum assisted resin transfer molding, differential scanning calorimetry, thermogravimetric analysis, scanning electron microscopy, fractographic analysis, cohesive failure, adhesive bonding, polymer matrix degradation, room temperature polymerization, composite joint mechanics
News Source: Denise Maddox. (November 26, 2026). Infrared Welding Efficiently Joins Recyclable Acrylic Composites Without Chemical Surface Preparation. Scienmag.